Used in the hand-layup process for various composite products, such as the manufacture and reinforcement of integral structural components and hulls for products like wind turbine blades and yachts.
It cures rapidly at low temperatures, achieving a cure rate of over 60% within 24 hours at low temperatures, allowing for sanding, load-bearing, and other operations.
Fast-curing and slow-curing hardeners can be freely mixed to achieve the desired curing speed.
Winter and summer resin formulations minimize the impact of temperature fluctuations on viscosity.
Certified by German Lloyd’s Register (GL).
| LT-5089 | Value | Remarks | Reference Standard |
| Mixing Viscosity | 25°C 800–2000 cps | Cast Body | GB/T 22314-2008 |
| Tg | >70°C | GB/T 19466.2-2004 | |
| Flexural strength | 100–125 MPa | GB/T 1447-2005 | |
| Curing Conditions | 25°C × 6–24 h | ||
| Color | Light brown |